Inconel X750/2.4669/UNS N07750 Inconel X750 is a nickel-chromium alloy similar to Inconel 600 but made precipitation-hardenable by additions of aluminum and titanium. It has good resistance to corrosion and oxidation along with high tensile and creep-rupture properties at temperatures to 1300¡ãF (700¡ãC). Its excellent relaxation resistance is useful for high-temperature springs and bolts. Used in gas turbines, rocket engines, nuclear reactors, pressure vessels, tooling, and aircraft structures. Chemical Composition


Physical Properties

Mechanical Properties
 |
|
|
|
|