Incoloy 800/H/HT/1.4876/UNS N08800 |
| Add Time: 2013-8-27 15:31:40 Source: ×÷Õß: µã»÷Êý:2580 |
Incoloy 800 / H / HT/1.4876/UNS N08800 Incoloy 800, Incoloy 800H, and Incoloy 800HT is nickel-iron-chromium super alloys. When exposed to high-temperature these alloys not only provide excellent resistance to oxidation and carburization but also good strength too. These nickel steel alloys are similar except for the higher level of carbon in Incoloy 800H, and the addition of up to 1.20 percent titanium and aluminum in Incoloy 800HT.
 |
|
|
|
|