Incoloy Alloy 28/N08028/Sanicro 28/1.4563-ASTM B668 |
| Add Time: 2013-8-27 16:15:37 Source: ×÷Õß: µã»÷Êý:2600 |
Incoloy Alloy 28/N08028/Sanicro 28/1.4563-ASTM B668 Alloy 28 (UNS N08028, W. Nr. 1.4563) is a nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localise attack such as pitting and crevice corrosion. The alloy is especially resistant to sulphuric and phosphoric acid. Used for chemical processing, pollution control equipment, oil and gas well piping, nuclear fuel reprocessing, acid production and pickling equipmen

|
|
|
|
|