1.4980/A286/ASTM A453 GR660 |
| Add Time: 2013-8-27 17:00:10 Source: ×÷Õß: µã»÷Êý:2459 |
1.4980/A286/ASTM A453 GR660 Alloy 286, also known as 660. Alloy 286 is a precipitation hardened austentic iron based steel, suitable for applications requiring high strength, good corrosion resistance at temperatures up to 700¡ãC, and a high degree of uniformity in developing full strength.Alloy 286 can be used in a wide range of high temperature applications, fasteners, and turbines, critical frames in high stress/heat applications, castings and fasteners. Chemical Composition


|
|
|
|
|