Add: No8 Jingyi Road,Sihong
SuQian, JiangSu China 223900
Tel: 86-(0)527-80686558
Sole Subsiciary:
Jiangsu ZSA Industry Co., Ltd.
SGS Certificated:CN22/20138
|
|
 |
|
|
| NEWS |
 |
|
| Add Time: 2013-9-2 13:51:55 Source: ×÷Õß: µã»÷Êý:3028 |
SS321/UNS S32100/1.4541 Stainless 321 is a heat resistant, titanium stabilized, austenitic alloy that's commonly used for service in the 1000¡ã-1600¡ãF temperature range. 321 stainless is primarily used in applications that involve continuous and intermittent service temperatures within the carbide precipitation range of 800¡ã-1500¡ãF. The steel has excellent forming and welding qualities and excellent toughness even at cryogenic temperatures. If you are looking for a stainless steel to provide resistance to intergranular corrosion, 304L is the normal choice as it is a more commonly used and supplied steel

|
|
|
|
|