SS347/UNS S34700/1.4550 Type 347 is a columbium/tantalum stabilized austenitic chromium-nickel stainless steel which was developed to provide an 18-8 type alloy with improved intergranular-corrosion resistance. Type 347 is stabilized against chromium carbide formation by the addition of columbium and tantalum. Since columbium and tantalum have a stronger affinity for carbon than chromium, columbium-tantalum carbides precipitate within the grains instead of forming at the grain boundaries. Type 347 should be considered for applications requiring intermittent heating between 800ºF (427ºC) and 1650ºF (899ºC), or for welding under conditions which prevent a post-weld anneal.

|
|
|
|
|