A193B6-6 STUD


SS410/UNS S41000/1.4006 Stainless steel 410 is a basic martensitic grade offering both exceptional wear and corrosion resistance. Elevated mechanical properties and corrosion resistance are achieved with stainless steel 410 when it's hardened and tempered. 410 stainless steel is used in applications such as dental and surgical instruments, pipelines, valves and nozzles, automotive parts and more. Please contact Best Stainless for more information about 410 SS, its properties, and its applications.

| |
|
|
|
|